Bigredwelder

  • Offline Rock Crawl'n
  • **
  • Turtle Points: -20
  • Male Posts: 67
  • Member since Apr '11
    • View Profile
Re: Need welding input/advice?
« on: Apr 10, 2011, 07:51:32 AM »
Ya the " stacked dime" look is stupid, craters like the moon, and cracking, I weld with c02 at home, hot and fast, no bead look at all, it flat and smooth. But when you weld right with a continues bead, and a certain gas, you will get ripples and have that effect which is fine. Just triggering it in, to get that is stupid.

 :thumbs:  Couldn't agree with ya more!  I also run 100% CO2 at home.  Its cheap and runs hotter.  Has more splatter than 75/25 or 85/15 but all around, it works pretty good.
Tungsten isn't filler material!  Quit dippin' it!


Some people are like a slinky....not really good for anything, but they sure can make you smile when you shove them down the stairs!

 
 
 
 
 

Related Topics

Welding advice
30 Replies
5806 Views
Last post Jan 31, 2005, 05:54:50 PM
by yotaboy79
27 Replies
4898 Views
Last post Feb 14, 2008, 02:08:28 AM
by 94MtnYote
34 Replies
10981 Views
Last post May 02, 2009, 12:24:47 PM
by Sparkplug
4 Replies
2038 Views
Last post Jan 07, 2011, 02:11:42 PM
by Thomas P
2 Replies
959 Views
Last post Mar 17, 2015, 08:51:43 PM
by helipilot77